Sphärische Metallpulver GH4169 Pulver auf Nickelbasis

Produktcharakter:

GH4169 is an aging precipitation strengthened alloy with γ~Ni as the matrix, γ ” phase (Ni3Nb) as the main phase, and weak strengthening phase γ ‘[Ni3 (Al, Ti)] with a face centered cubic structure. It has excellent high-temperature strength, oxidation resistance, corrosion resistance, fatigue resistance, and good high-temperature creep strength. It is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.

Markenname Jinchun
Herkunft China
Name des Produkts GH4169 powder
Anmeldung Hot end structural components  in aerospace, energy, military and other fields.
Form Pulver
Farbe Metal gray
Größe 15~53μm
Standard GB/T 19001-2016/ISO9001: 2015
Reinheit  Ni: 50-55%, Cr:17-21%, Mo:2.8-3.3%, Nb: 4.75-5.50%, Ti:0.65-1.15%, Fe: Bal.
Material Ni, Cr, Mo, Nb, Ti, Fe
Verpacken Vakuumverpackung
Produkt Charakter GH4169 is an aging precipitation strengthened alloy with γ~Ni as the matrix, γ ” phase (Ni3Nb) as the main phase, and weak strengthening phase γ ‘[Ni3 (Al, Ti)] with a face centered cubic structure. It has excellent high-temperature strength, oxidation resistance, corrosion resistance, fatigue resistance, and good high-temperature creep strength. It is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.   2.Spezifikation GH4169 powder
Chemische Zusammensetzung (wt.%)
Element C Cr Ni Co Mo Al Ti Fe B
Standard ≤0.08 17.0~21.0 50.0~55.0 ≤1.0 2.8~3.3 0.2~0.8 0.65~1.15 Bal. ≤0.006
typisch 0.078 18.97 52.98 0.005 3 0.65 1.1 Bal. 0.005
Element Mn P S Cu Mg Si Nb O N
Standard ≤0.35 ≤0.05 ≤0.015 ≤0.30 ≤0.01 ≤0.35 4.75~5.50 ≤0.030 ≤0.030
typisch 0.33 0.009 0.0078 0.0039 0.002 0.32 5.02 0.017 0.01
 
GH4169 15~53μm Partikelgrößenverteilung Durchflussrate (sec. für 50 g) Scheinbare Dichte (g/cm3) Klopfdichte (g/cm3)
D10 D50 D90
Standard 15~25 30~40 50~60 ≤25 ≥4.2 ≥4.9
typisch 22.3μm 34.9μm 53.3μm 17 4.22 4.93
  3 Bilder der SEM-Morphologie des Pulvers Bilder von Produktion und Test:   4.Anwendung
  • GH4169  powder is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.

5. qualitätssicherung

Hinterlassen Sie Ihre Nachricht