Caractéristiques du produit:
Jinchun provides carbonyl iron powder in food grade and industrial grade with different sizes and purities.
Nom de la marque | Jinchun |
Origine | Chine |
Nom du produit | Poudre de fer carbonique |
Application | Animal feed, nutritional iron supplement, soft Magnetic field iron powder core, chip inductor, printing ink, etc. |
Forme | Poudre |
Couleur | Metal gray |
Taille | D50: 2.0-3.0μm, 4.5-6.5μm, 4.5-6.5μm |
Standard | GB/T 19001-2016/ISO9001 : 2015 |
La pureté | Fe: 98%, 99% |
Matériau | Iron. |
Emballage | Tambours d'acier |
Jinchun provides carbonyl iron powder in food grade and industrial grade with different sizes and purities.
2.Specification for Food gradeName: Carbonyl Iron Powder food grade | Spec: | ||
Chemical Composition: | Size:Micron | ||
Fe | 98.38% (97.8%min) | O | 0.22% (0.40%max) |
C | 0.616% (0.80max) | N | 0.48%(0.6%max) |
Apparent Density(g/cm3) | 2.67(2.50min) | Tap Density(g/cm3) | 4.47(3.90min) |
Size Distribution | D10 | 0.8-2.0 | 1.14 |
D50 | 2.0-3.0 | 2.41 | |
D90 | 4.0-18.0 | 6.19 |
The application of carbonyl iron powder Food Grade
Food grade carbonyl iron powder is mainly used in animal feed and nutritional iron supplement in European and American countries. The main index of the product is that the content of heavy metals meets the European Union standard. The heavy metals in our products only contain nickel. Through process adjustment, it has been in line with the European Union animal feed and nutritional iron supplement.
3. Specification for Industrial gradeNom/ Type | Chemical Components (%) | Pysical Poperty | Battery prformance | ||||||||
Fe | C | N | O | Apparent density | Tap density | Size(D50) | Permeability | Q Value | DC superimposed inductance drop(12.8A) | Insulation resistance(MΩ/DC100V) | |
JCF4-4 | Bal. | ≤0.05% | ≤0.01 | ≤0.6 | ≥2.5 | ≥3.8 | 3.5-5.5 | 34-38 | 110-130 | ≤4% | ≥1000 |
JCF4-5 | Bal. | ≤0.05% | ≤0.01 | ≤0.6 | ≥2.5 | ≥3.8 | 4.5-6.5 | 36-41 | 100-120 | ≤5% | ≥1000 |
Nom/ Type | Élément | Fe | C | O | N |
JCF4-6 | Résultat(%) | 98.02 | 0.51 | 0.34 | 0.60 |
Nom/ Type | Élément | Fe | C | O | N |
JCF4-7 | Résultat(%) | 99.53 | 0.033 | 0.27 | 0.010 |
1. Sample forming conditions: sample powder plus 1% epoxy resin, 21t pressing molding, 160 ℃ curing for 1.5h
2. Magnetic ring size: outer diameter 26.9mm, inner diameter 14.5mm, height 10-11mm
3. Filling amount: :27.5±0.05g
4. Inductance test condition: 10KHz 0.02V 12.8A
5. Requirements for inductance test: φ0.4mm,N=20
6. DC superposition test conditions:10KHz 0.02V 12.8A
7. DC superposition requirements: φ0.8mm,N=20
8. Printing ink.
4.SEM photos of carbonyl iron powder industrial grade