Chengdu Jinchun Metallic Materials Co, Ltd.

Poudres métalliques sphériques GH3536 Superalloy Poudre d'alliage haute température

Caractéristiques du produit:

GH3536 high-temperature alloy is a nickel based alloy with high iron content that has been solid solution strengthened with Cr and Mo elements high temperature alloy, which has good corrosion resistance and oxidation resistance, can be used for a long time at 900 ℃, suitable for manufacturing combustion chamber components of aircraft engines with a short-term working temperature of 1080 ℃ other high-temperature components.

Nom de la marque Jinchun
Origine Chine
Nom du produit GH3536 powder
Application Combustion chamber components of aircraft engines and other high-temperature components.
Forme Poudre
Couleur Gris métal
Taille 15~53μm
Standard GB/T 19001-2016/ISO9001 : 2015
La pureté  Ni: Bal.  Cr: 20.5-23.0%, Mo:8.0-10.0%, Co:0.5-2.5%,Fe: 17.0-20.0%
Matériau Ni, Cr, Mo, Co, Fe
Emballage Emballage sous vide
Caractère du produit GH3536 high-temperature alloy is a nickel based alloy with high iron content that has been solid solution strengthened with Cr and Mo elements high temperature alloy, which has good corrosion resistance and oxidation resistance, can be used for a long time at 900 ℃, suitable for manufacturing combustion chamber components of aircraft engines with a short-term working temperature of 1080 ℃ other high-temperature components.   2. cahier des charges GH3536powder
Composition chimique (wt.%)
Élément C Cr Ni Co Mo Al Ti Fe B
Standard 0.05~0.15 20.5~23.0 Bal. 0.5~2.5 8.0~10.0 ≤0.50 ≤0.15 17.0~20.0 ≤0.010
typique 0.08 21.94 Bal. 1.42 8.97 0.14 0.012 18.98 0.002
Élément Mn P S Cu W Si O N
Standard ≤1.0 ≤0.025 ≤0.015 ≤0.50 0.2-1.0 ≤1.0 ≤0.030 ≤0.030
typique 0.26 0.005 0.005 0.007 0.55 0.34 0.017 0.024
 
GH3536 15~53μm Distribution de la taille des particules Débit (sec. pour 50 g) Densité apparente (g/cm3) Densité (g/cm3)
D10 D50 D90
Standard 15~25 30~40 50~60 ≤25 ≥4.2 ≥4.9
typique 23.4μm 36.2μm 55.2μm 20 4.24 5.03
  3.Images de la morphologie de la poudre au microscope électronique à balayage Photos de la production et des essais :   4.Application
  • GH3536  powder  is applied in combustion chamber components of aircraft engines and other high-temperature components.

5. l'assurance qualité