Jinchun provides carbonyl iron powder in food grade and industrial grade with different sizes and purities.
ブランド名 | ジンチュン |
起源 | 中国 |
商品名 | カルボニル鉄粉 |
申し込み | Animal feed, nutritional iron supplement, soft Magnetic field iron powder core, chip inductor, printing ink, etc. |
形状 | パウダー |
カラー | Metal gray |
サイズ | D50: 2.0-3.0μm, 4.5-6.5μm, 4.5-6.5μm |
スタンダード | GB/T 19001-2016/ISO9001: 2015 |
純度 | Fe: 98%, 99% |
素材 | Iron. |
梱包 | スチールドラム |
Jinchun provides carbonyl iron powder in food grade and industrial grade with different sizes and purities.
2.Specification for Food gradeName: Carbonyl Iron Powder food grade | Spec: | ||
Chemical Composition: | Size:Micron | ||
フェ | 98.38% (97.8%min) | O | 0.22% (0.40%max) |
C | 0.616% (0.80max) | N | 0.48%(0.6%max) |
Apparent Density(g/cm3) | 2.67(2.50min) | Tap Density(g/cm3) | 4.47(3.90min) |
Size Distribution | D10 | 0.8-2.0 | 1.14 |
D50 | 2.0-3.0 | 2.41 | |
D90 | 4.0-18.0 | 6.19 |
The application of carbonyl iron powder Food Grade
Food grade carbonyl iron powder is mainly used in animal feed and nutritional iron supplement in European and American countries. The main index of the product is that the content of heavy metals meets the European Union standard. The heavy metals in our products only contain nickel. Through process adjustment, it has been in line with the European Union animal feed and nutritional iron supplement.
3. Specification for Industrial grade名前/タイプ | Chemical Components (%) | Pysical Poperty | Battery prformance | ||||||||
フェ | C | N | O | Apparent density | Tap density | Size(D50) | Permeability | Q Value | DC superimposed inductance drop(12.8A) | Insulation resistance(MΩ/DC100V) | |
JCF4-4 | バル | ≤0.05% | ≤0.01 | ≤0.6 | ≥2.5 | ≥3.8 | 3.5-5.5 | 34-38 | 110-130 | ≤4% | ≥1000 |
JCF4-5 | バル | ≤0.05% | ≤0.01 | ≤0.6 | ≥2.5 | ≥3.8 | 4.5-6.5 | 36-41 | 100-120 | ≤5% | ≥1000 |
名前/タイプ | エレメント | フェ | C | O | N |
JCF4-6 | 結果(%) | 98.02 | 0.51 | 0.34 | 0.60 |
名前/タイプ | エレメント | フェ | C | O | N |
JCF4-7 | 結果(%) | 99.53 | 0.033 | 0.27 | 0.010 |
1. Sample forming conditions: sample powder plus 1% epoxy resin, 21t pressing molding, 160 ℃ curing for 1.5h
2. Magnetic ring size: outer diameter 26.9mm, inner diameter 14.5mm, height 10-11mm
3. Filling amount: :27.5±0.05g
4. Inductance test condition: 10KHz 0.02V 12.8A
5. Requirements for inductance test: φ0.4mm,N=20
6. DC superposition test conditions:10KHz 0.02V 12.8A
7. DC superposition requirements: φ0.8mm,N=20
8. Printing ink.