製品特性:...
GH4099 is a typical aging strengthened nickel based high-temperature alloy, which is comprehensively strengthened with elements such as Co, W, Al, Ti, etc., giving the alloy high thermal strength. It can be used for a long time below 900 ℃, and the highest working temperature can reach 1000 ℃. Due to its stable microstructure and satisfactory cold and hot forming and welding process performance, GH4099 high-temperature alloy is very suitable for manufacturing high-temperature plate load-bearing welding structures such as aviation engine combustion chambers and afterburner chambers.
ブランド名 | ジンチュン |
起源 | 中国 |
商品名 | GH4099 powder |
申し込み | High-temperature plate load-bearing welding structures, etc. |
形状 | パウダー |
カラー | Metal gray |
サイズ | 15~53μm |
スタンダード | GB/T 19001-2016/ISO9001: 2015 |
純度 | Ni: Bal. , Cr:17-20%, Mo:3.5-4.5%, Co: 5.0-8.0%, W:5.0-7.0%, Al: 1.7-2.4%, Ti: 1-1.5%. |
素材 | Ni, Cr, Mo, W, Ti, Al, Co |
梱包 | 真空包装 |
化学組成 (wt.%) | |||||||||
エレメント | C | Cr | ニー | Co | W | モ | ティ | フェ | B |
スタンダード | ≤0.08 | 17.0~20.0 | バル | 5.0~8.0 | 5.0~7.0 | 3.5~4.5 | 1.0~1.5 | ≤2.0 | ≤0.005 |
typical | 0.031 | 18.08 | バル | 6.38 | 5.99 | 4.07 | 1.21 | 0.084 | 0.004 |
エレメント | ムン | P | S | アル | Mg | Si | Ce | O | N |
スタンダード | ≤0.40 | ≤0.015 | ≤0.015 | 1.7~2.4 | ≤0.01 | ≤0.50 | ≤0.02 | ≤0.030 | ≤0.030 |
typical | 0.03 | 0.006 | 0.00063 | 2.01 | 0.001 | 0.1 | 0.006 | 0.0072 | 0.017 |
GH4099 | 15~53μm 粒度分布 | 流量 秒(50gの場合) | 見掛け密度(g/cm3) | タップ密度(g/cm3) | ||
D10 | D50 | D90 | ||||
スタンダード | 15~25 | 30~40 | 50~60 | ≤25 | ≥4.2 | ≥4.9 |
typical | 22.2μm | 35.5μm | 54.3μm | 16.2 | 4.58 | 5.26 |