成都金春金属材料有限公司

球状金属粉末 GH4169 ニッケル基粉末

製品特性:...

GH4169 is an aging precipitation strengthened alloy with γ~Ni as the matrix, γ ” phase (Ni3Nb) as the main phase, and weak strengthening phase γ ‘[Ni3 (Al, Ti)] with a face centered cubic structure. It has excellent high-temperature strength, oxidation resistance, corrosion resistance, fatigue resistance, and good high-temperature creep strength. It is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.

ブランド名 ジンチュン
起源 中国
商品名 GH4169 powder
申し込み Hot end structural components  in aerospace, energy, military and other fields.
形状 パウダー
カラー Metal gray
サイズ 15~53μm
スタンダード GB/T 19001-2016/ISO9001: 2015
純度  Ni: 50-55%, Cr:17-21%, Mo:2.8-3.3%, Nb: 4.75-5.50%, Ti:0.65-1.15%, Fe: Bal.
素材 Ni, Cr, Mo, Nb, Ti, Fe
梱包 真空包装
製品キャラクター GH4169 is an aging precipitation strengthened alloy with γ~Ni as the matrix, γ ” phase (Ni3Nb) as the main phase, and weak strengthening phase γ ‘[Ni3 (Al, Ti)] with a face centered cubic structure. It has excellent high-temperature strength, oxidation resistance, corrosion resistance, fatigue resistance, and good high-temperature creep strength. It is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.   2.仕様 GH4169 powder
化学組成 (wt.%)
エレメント C Cr ニー Co アル ティ フェ B
スタンダード ≤0.08 17.0~21.0 50.0~55.0 ≤1.0 2.8~3.3 0.2~0.8 0.65~1.15 バル ≤0.006
typical 0.078 18.97 52.98 0.005 3 0.65 1.1 バル 0.005
エレメント ムン P S Mg Si Nb O N
スタンダード ≤0.35 ≤0.05 ≤0.015 ≤0.30 ≤0.01 ≤0.35 4.75~5.50 ≤0.030 ≤0.030
typical 0.33 0.009 0.0078 0.0039 0.002 0.32 5.02 0.017 0.01
 
GH4169 15~53μm 粒度分布 流量 秒(50gの場合) 見掛け密度(g/cm3) タップ密度(g/cm3)
D10 D50 D90
スタンダード 15~25 30~40 50~60 ≤25 ≥4.2 ≥4.9
typical 22.3μm 34.9μm 53.3μm 17 4.22 4.93
  3.粉末のSEM形態写真 生産とテストの写真:   4.申し込み
  • GH4169  powder is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.