製品特性:...
GH4169 is an aging precipitation strengthened alloy with γ~Ni as the matrix, γ ” phase (Ni3Nb) as the main phase, and weak strengthening phase γ ‘[Ni3 (Al, Ti)] with a face centered cubic structure. It has excellent high-temperature strength, oxidation resistance, corrosion resistance, fatigue resistance, and good high-temperature creep strength. It is commonly used in the manufacture of hot end structural components and is widely used in aerospace, energy, military and other fields.
ブランド名 | ジンチュン |
起源 | 中国 |
商品名 | GH4169 powder |
申し込み | Hot end structural components in aerospace, energy, military and other fields. |
形状 | パウダー |
カラー | Metal gray |
サイズ | 15~53μm |
スタンダード | GB/T 19001-2016/ISO9001: 2015 |
純度 | Ni: 50-55%, Cr:17-21%, Mo:2.8-3.3%, Nb: 4.75-5.50%, Ti:0.65-1.15%, Fe: Bal. |
素材 | Ni, Cr, Mo, Nb, Ti, Fe |
梱包 | 真空包装 |
化学組成 (wt.%) | |||||||||
エレメント | C | Cr | ニー | Co | モ | アル | ティ | フェ | B |
スタンダード | ≤0.08 | 17.0~21.0 | 50.0~55.0 | ≤1.0 | 2.8~3.3 | 0.2~0.8 | 0.65~1.15 | バル | ≤0.006 |
typical | 0.078 | 18.97 | 52.98 | 0.005 | 3 | 0.65 | 1.1 | バル | 0.005 |
エレメント | ムン | P | S | 銅 | Mg | Si | Nb | O | N |
スタンダード | ≤0.35 | ≤0.05 | ≤0.015 | ≤0.30 | ≤0.01 | ≤0.35 | 4.75~5.50 | ≤0.030 | ≤0.030 |
typical | 0.33 | 0.009 | 0.0078 | 0.0039 | 0.002 | 0.32 | 5.02 | 0.017 | 0.01 |
GH4169 | 15~53μm 粒度分布 | 流量 秒(50gの場合) | 見掛け密度(g/cm3) | タップ密度(g/cm3) | ||
D10 | D50 | D90 | ||||
スタンダード | 15~25 | 30~40 | 50~60 | ≤25 | ≥4.2 | ≥4.9 |
typical | 22.3μm | 34.9μm | 53.3μm | 17 | 4.22 | 4.93 |