Carácter do produto
The reduction process is divided into (solid carbon reduction) primary reduction and secondary reduction. The primary reduction is the production of sponge iron by solid carbon reduction. The main process of primary reduction is: (iron concentrate, rolled steel scales, etc.) → drying → magnetic separation → crushing → screening → canning → entering the primary reduction furnace → sponge iron. Secondary precision reduction process: Sponge iron → Cleaning → Crushing → Magnetic separation → Secondary reduction furnace → Powder block → Crushing → Magnetic separation → Screening → Grading → Mixing → Packaging → Finished product.
1.Specification
Reduced iron powder FHT40.30, FHT40.37, FHT100.25
Nome/tipo |
Elemento |
Fe |
C |
Si |
Mn |
P |
S |
H Loss |
Reduced iron powder |
Padrão(%) |
>98.5 |
<0.03 |
<0.10 |
<0.30 |
<0.030 |
<0.030 |
<0.030 |
Resultado(%) |
98.70 |
0.013 |
0.08 |
0.08 |
0.010 |
0.016 |
0.25 |
2.Pictures of Raw Materials and Production
Imagens de produção:
3.Aplicação
High strength structural components in powder metallurgy, pharmaceutical and chemical industries, chemical catalysts, hard alloys, diamond tools, soft magnetic powder parts, rubber resin products, welding materials, metal smelting, environmental protection industry, daily necessities industry, food industry and other industries.